The uneven appearance of the paint coating, which resembles the peel of an orange or walnut, is called orange peel.
The reasons are as follows:
1) The construction viscosity is too high and the paint film leveling is poor;
2) Improper selection of spray gun;
3) High temperature and low humidity in the spray room;
4) Insufficient leveling time and premature entry into the drying room;
5) Spraying film is too thick or too thin
Solutions:
1) Add pure water to adjust the coating viscosity;
2) Standardize the spray gun, or adjust the spraying distance, fan width, etc.;
3) Reduce the temperature of the spray room, improve the humidity of the spray room;
4) Increase leveling time;
5) Adjust the amount of spit and gun speed to prevent the paint film thickness beyond the specified range.
Short comments: in the process of painting epoxy phenolic drum closures, the orange peel probelm will also occur, but with small probability, we will check each closures for customers.
Spot Market For ScarpJuly 1, 2022Scrap: On April 8, the scrap market price continued to run strongly, the average price of scrap steel in 45 major markets in the country was 3030 yuan/ton, up 18 yuan/ton compared with the last tradin...view
Flange in Blocked TankJune 19, 2023Today we will mainly introduce the flange in the drum closure, which is made of cold-rolled steel and is divided into 2-inch and 4/3-inch sizes for standard 55-gallon stainless steel drums. The surfac...view
Packaging Market And Development Trends In North AmericaJuly 1, 2022North America is the world's second largest packaging market after China. As of 2017, the apparent packaging consumption in North America was approximately US$2030 billion. Although packaging in N...view
Overview Of National Packaging Industry Operation In 2020July 1, 2022In 2020, there will be 8,183 enterprises above scale in China's packaging industry (all industrial legal person enterprises with an annual revenue of 20 million yuan or above), 267 more than last ...view